Zirconium dioxide (ZrO2) is often called as zirconia in industries, it is a white crystalline oxide of zirconium. It is one of the most studied and used ceramic materials. This material and its products have excellent physical characteristics and unique chemical properties. It has three phases with monoclinic below 1170 °C, tetragonal between 1170 °C and 2370 °C, and cubic above 2370 °C.
Pure ZrO2 indicates a monoclinic crystal structure at room temperature and will transition to tetragonal and cubic at successive higher temperatures. The mostly popular used zirconia is that of tetragonal zirconia polycrystal (TZP), which is indicative of polycrystalline zirconia composed of only metastable tetragonal phase. When zirconia is mixed with some additives, both the tetragonal and cubic phases are partially stabilized. Effective stabilizers include yttrium oxide (Y2O3, yttria), magnesium oxide (MgO), calcium oxide (CaO) and ceriumoxide (Ce2O3). They are usually called Y-PSZ, Mg-PSZ, Ca-PSZ and Ce-PSZ.
Zirconia Ceramic Pins And Plugs |
Zirconia Ceramic Plugs |
Zirconia Ceramic Pins |
Shanghai Fine-boon is a professional ceramic supplier that integrates design, molding, sintering, production, machining and sales of precision ceramic products from 2004. Through decades of fast developing, we accumulated abundant experiences, extensive knowledge, and advanced production equipments for various industrial ceramic production. We can provide not only finished zirconia pins and plugs, but also professional ceramic solutions for your upgrading demands. No matter easy pins or complex plugs, we can submit to you with just-in-time delivery for tailor-made zircon pins and plugs. Our zirconia locating pins for welding machines have proved to be a really reliable pin for mass production use.
As a reliable ceramic specialist, we clearly understand the quality importance for our customers. Quality is the foundation for the success of our ceramic business. We got strict quality control for all our ceramic pins and plugs through our production. We also get senior inspectors and various advanced inspection equipments for 100% inspection for each zirconia pins and plugs before delivery. This will ensure that all our zirconia pins and plugs are defect-free and perfect for your assembly use.
Product Name | Customized Zirconia Ceramic Pins and Plugs with High Precision |
Compositions |
94.7% ZrO2 + 5.2% Y2O3 in weight percentage |
Color |
White |
Density |
6.0 g/cm3 |
Tolerance |
+/- 0.005mm |
Finishing |
Ra 0.02 with Micro lapping and Fine-polishing |
Max. Using Temperature |
1300 ℃ |
Using Fields |
Various Advanced Pumps and Motor, Fans and Ventilation Equipments, Spot Welding Machines |
The Strength for Our Zirconia Pins and Plugs:
- Robust physical characteristics, 3-6 times better than alumina
- Unique transformation toughening to anti-crack
- Good wear resistance for long time use
- High precision and fine polished surface
- Self-lubricating and maintenance-free
- Good insulation, anti-magnetic, static electricity-free character
- Excellent chemical stability for chemical plants use
- Outstanding corrosion resistance in harsh environments
- Good thermal stability and anti high-temperature creeping
- Non-toxic, healthy material
- Conform to ROHS and REACH regulations, environmental friendly
- Turnkey project managing with one stop service
Zirconia Ceramics Properties Sheet | |||
- Shanghai Fine-Boon | |||
Properties |
Unit |
Y-PSZ Zirconia Partially stable zirconia (added zirconium oxide) |
Y-FSZ Zirconia Fullstable zirconia (added zirconium oxide) |
ZrO2 Contents |
wt-% |
≥94 |
86 |
Y2O3 Contents |
wt-% |
5.2 |
14 |
Melting Point |
℃ |
- |
≥2500 |
Max. use Temperature |
℃ |
1300 |
2200 |
Color |
White |
White |
|
Density |
g /cm3 |
6 |
5.8 |
Flexural Strength |
MPa ≥ |
1000 |
200 |
Elastic Modulus(Young) |
GPa |
320 |
200 |
Hardness (HRA) |
HRA ≥ |
90 |
86 |
Coeff. of Thermal expansion |
×10-6/℃ |
10 |
8-10 |
Thermal Conductivity |
W/m·K( 20℃) |
2.6 |
1-2 |
Dielectric constant(1MHz25℃) |
33 |
12 |
|
Volume Resistivity |
Ω·cm 20℃ |
1014 |
109 |
Gas-tightness |
Pass |
Pass |
|
Thermal shock Resistance |
Pass |
Pass |
|
Dielectric Strength |
kV/mm , DC≥ |
20 |
- |
Acid Resistance (10% HCL mg/cm3) |
mg/cm2 ≤ |
2 |
5.5 |
Alkali Resistance (1:9 NaOH mg/cm3) |
mg/cm2 ≤ |
0.08 |
0.16 |
Wear Ability |
g/cm2 ≤ |
0.05 |
- |
Compressive Strength |
MPa ≥ |
2000 |
2200 |
Tensile Strength |
MPa ≥ |
600 |
- |